全國熱線服務(wù):
新聞資訊 Top label
- The Complete Guide to Pressure Sensors: Technology, Applications, and Selection Criteria
- The Evolution and Advantages of Electro-Hydraulic Synchronous Press Brakes in Modern Manufacturing
- Revolutionizing Semiconductor Manufacturing: The Role of Electrostatic Chucks in Modern Wafer Processing
- What Is A Humidity Sensor? How Does It Affect Our Lives And Work?
- The Essential Guide to Modern Bending Machines: Technology, Applications, and Selection Criteria
- The Complete Guide to Modern Hospital Beds: Transforming Patient Care Through Advanced Design
How to avoid scratches when cold drawn pipe is re-rolled
After analysis, it was found that such regular scratches on the cold drawn pipe may be caused by mis-layering. In order to improve this situation, we instead use rough roller rolling or smoothing to increase the inter-layer friction coefficient of the steel coil, thereby reducing the possibility of mis-layering scratches.
Since the rewinding is carried out after the flattening process, the outlet purge system of the flattening machine can be improved. This can reduce the remaining impurities on the surface of the product and avoid scratches. In addition, after we refuel the reel, it is best to perform multiple expansion and contraction operations before installing the sleeve. The purpose of this is to prevent the sleeve from being overstrained before use, thereby affecting the processing quality of the cold drawn tube.